I've seen several unfavorable comments over the years, mostly having
to do with issues in removing it to replace the stuff.

You can get the Gore material at any good industrial supply...at half
the price of marine stores....they use it in industry for valve
packing.

On Tue, Apr 26, 2011 at 7:53 AM, jim brown <jbrown5093 at yahoo.com> wrote:
> Anyone have experience with the putty like teflon packing material sold by West
> Marine and others. Seems like an easy way to go-almost too easy.
>
>
> Jim Brown
>
>
>
>
> ________________________________
>



-- 
Chris Burti
Farmville, NC